7612 جودة مواصفات الورقة
General application steels for drawing (automotive, refrigerators, washing machines, home appliances, etc)
رموز الحروف القابلة لإعادة الإنتاج --> CCR --> CCRD --> CCRF --> CCRFS --> CCR
Flat / Cold Rolled
Cold rolled coils or flat steel products are produced by rolling hot rolled flat steels without a heat treatment operation in a thickness range of 0.20 to 2.00mm. While the product’s physical properties are all homogeneous along the strip, surface flatness, width and thickness values have fulfilled expectations at the top level.
General application steels for drawing (automotive, refrigerators, washing machines, home appliances, etc)
التركيب الكيميائي (%)
| المعيار المكافئ | رقم جودة إرديمير | Cmax. | Mnmax. | Pmax. | Smax. | Bmin. | Bmax. | |
|---|---|---|---|---|---|---|---|---|
| المعيار | جودة | |||||||
| EN 10130:2006 | DC01 | 7612 | 0.12 | 0.60 | 0.045 | 0.045 | 20.00 | 50.00 |
- Suitable for welding of electric-resistance.
- The B limit is specified as reference value according to Erdemir manufacturing practice. Other limits are customer specification limits.
الخواص الميكانيكية
| المعيار المكافئ | رقم جودة إرديمير | Re [N/mm2] t(thickness, mm) | Rm [N/mm2] | A(%) min. t(thickness, mm) | |||||
|---|---|---|---|---|---|---|---|---|---|
| المعيار | جودة | ||||||||
| 0.2≤t≤0.5 | 0.51≤t≤0.7 | 0.71≤t≤2 | A800.2≤t≤0.5 | A800.51≤t≤0.7 | A800.71≤t≤2 | ||||
| EN 10130:2006 | DC01 | 7612 | 320 max. | 300 max. | 280 max. | 270-410 | 24 | 26 | 28 |
- Tensile test values apply to "transverse" test pieces
- For design purposes, the lower limit of Re may be assumed to be 140 N/mm² (14,3 kg/mm²)
- The upper limit Re of 280 Mpa is valid only for 8 days from the time of the availability of the product and recomended that the products should be formed within 6 weeks from the time of their availability.
- The guarantee period of absence of stretcher strains marks is 3 months for B surface quality products.