9461 جودة مواصفات الورقة
İnce taneli kaynaklanabilir yapı çeliği
البدائللا يوجد بديل لهذه الورقة.
Flat / Plate
Heavy plate products are obtained by rolling semi-finished products with a rectangular cross-section (slab) produced by the continuous casting method to a specific temperature, with thicknesses ranging from 6.00 to 200.00 mm and widths ranging from 1000 to 3600 mm.
İnce taneli kaynaklanabilir yapı çeliği
التركيب الكيميائي (%)
| المعيار المكافئ | رقم جودة إرديمير | Cmax. | Mnmin. | Mnmax. | Pmax. | Smax. | Simax. | Almax. | Nmax. | Crmax. | Momax. | Nimax. | Vmax. | Nbmax. | Timax. | Cumax. | Ceq+C+Buyuk+012max. | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| المعيار | جودة | |||||||||||||||||
| EN 10025-3:2019 | S460NL | 9461 | 0.20 | 1.00 | 1.70 | 0.025 | 0.02 | 0.60 | 0.02 | 0.025 | 0.30 | 0.10 | 0.80 | 0.20 | 0.05 | 0.05 | 0.55 | 0.53 |
- The chemical composition of the steel contains sufficient amounts of nitrogen-binding elements, the minimum Al value does not apply.
- CEV (IIW) % = C + Mn / 6 + (Cr + Mo + V) / 5 + (Ni + Cu) / 15
- The maximum carbon equivalent (CEV) may be increased by 0.02% for Si ≤ 0.04% and by 0.01% for Si ≤ 0.25%.
- Production is carried out—subject to consultation—using special manufacturing conditions for thicknesses up to a maximum of 40 mm.
- V + Nb + Ti ≤ 0,22 % and Mo + Cr ≤ 0,30 %.
- Normalizing Rolling Method
- Normalizing Rolling Method
الخواص الميكانيكية
| المعيار المكافئ | رقم جودة إرديمير | Re [N/mm2] t(thickness, mm) | Impact | |||
|---|---|---|---|---|---|---|
| المعيار | جودة | |||||
| 16.01≤t≤40 | 40.01≤t≤60 | Temperature ( ° C) | KVC J min. | |||
| EN 10025-3:2019 | S460NL | 9461 | 440 min. | 430 min. | -50 | 27 |
- Tensile test values apply to "transverse" test pieces
- Impact tests are not performed on products with a thickness of less than 6 mm.