482 Quality Sheet Specification
Zinc-iron alloy coated (galvannealed) bake-hardening steels
Reproducible Letter Symbols --> GFR --> GFRD --> GFR
Flat / Galvanised
Galvanized flat steel is manufactured by zinc-coating both sides of cold rolled metal by hot-dipping process. After having coated the steel surface with zinc, the coating of the interface is transformed into an alloy of iron-zinc layer through heating by induction and the galvannealed steel is produced.
Zinc-iron alloy coated (galvannealed) bake-hardening steels
Chemical Composition (%)
| Standard Equivalent | Erdemir Grade No | Cmax. | Mnmax. | Pmax. | Smax. | Nbmax. | Timax. | |
|---|---|---|---|---|---|---|---|---|
| Standard | Quality | |||||||
| TSG3109G | SCGA 340BH | 482 | 0.008 | 0.70 | 0.08 | 0.02 | 0.04 | 0.05 |
- Chemical composition is not specified in customer specification. Limits given in this table are based on Erdemir practice for reference.
Mechanical Properties
| Standard Equivalent | Erdemir Grade No | Re [N/mm2] | Rm [N/mm2] | A(%) min. | rort | BH2 [N/mm2] min. | |
|---|---|---|---|---|---|---|---|
| Standard | Quality | ||||||
| A80 | |||||||
| TSG3109G | SCGA 340BH | 482 | 195-295 | 340 min. | 34-41 | 1.4 min. | 30 |
- Tensile test values apply to "transverse" test pieces
- BH value is obtained at 170°C in 20 minutes.
- Intended BH2 value is 40 N/mm2 (4.1 kg/mm2).
- Mechanical properties are guaranteed for thickness d = 0.70 mm.
- The mechanical properties are valid for a period of 3 months from the date on which the products are made available.