6113 Quality Sheet Specification
General application steels for drawing (automotive, refrigerators, washing machines, home appliances, etc)
Reproducible Letter Symbols --> CCR --> CCRD --> CCRF --> CCRFS --> CCR
Flat / Cold Rolled
Cold rolled coils or flat steel products are produced by rolling hot rolled flat steels without a heat treatment operation in a thickness range of 0.20 to 2.00mm. While the product’s physical properties are all homogeneous along the strip, surface flatness, width and thickness values have fulfilled expectations at the top level.
General application steels for drawing (automotive, refrigerators, washing machines, home appliances, etc)
Chemical Composition (%)
| Standard Equivalent | Erdemir Grade No | Cmax. | Mnmax. | Pmax. | Smax. | |
|---|---|---|---|---|---|---|
| Standard | Quality | |||||
| EN 10130:2006 | DC03 | 6113 | 0.10 | 0.45 | 0.035 | 0.035 |
- Deoxidation method of this products is fully-killed. Minimum aluminium to nitrogen ratio is 2:1.
- Can be produced with titanium added.
Mechanical Properties
| Standard Equivalent | Erdemir Grade No | Re [N/mm2] t(thickness, mm) | Rm [N/mm2] | A(%) min. t(thickness, mm) | r90 | |||||
|---|---|---|---|---|---|---|---|---|---|---|
| Standard | Quality | |||||||||
| 0.2≤t≤0.5 | 0.5≤t≤0.7 | 0.71≤t≤2 | A800.2≤t≤0.5 | A800.51≤t≤0.7 | A800.71≤t≤2 | |||||
| EN 10130:2006 | DC03 | 6113 | 280 max. | 260 max. | 240 max. | 270-370 | 30 | 32 | 34 | 1.3 min. |
- Tensile test values apply to "transverse" test pieces
- The value of r90 only apply to products of thickness d ≥ 0.5 mm.
- For design purposes, the lower limit of Re may be assumed to be 140 N/mm² (14,3 kg/mm²)
- Guarantee periods of absence of stretcher strains marks and mechanical properties are 6 months. The period begin on the date on which products are made available.