312 Quality Sheet Specification
Zinc coated (galvanized) low carbon steels for cold forming
Reproducible Letter Symbols --> GZR --> GZRD --> GZR
AlternativesThere is no alternative to this sheet.
Flat / Galvanised
Galvanized flat steel is manufactured by zinc-coating both sides of cold rolled metal by hot-dipping process. After having coated the steel surface with zinc, the coating of the interface is transformed into an alloy of iron-zinc layer through heating by induction and the galvannealed steel is produced.
Zinc coated (galvanized) low carbon steels for cold forming
Chemical Composition (%)
| Standard Equivalent | Erdemir Grade No | Cmax. | Mnmax. | Pmax. | Smax. | Simax. | Almin. | Almax. | CEmax. | |
|---|---|---|---|---|---|---|---|---|---|---|
| Standard | Quality | |||||||||
| 11-04-013 | XE | 312 | 0.08 | 0.50 | 0.025 | 0.025 | 0.04 | 0.005 | 0.07 | 0.16 |
- "CE = C % + (Mn+Si)/6 %" formula applies for carbon equivalent.
- The limits which are specified in the table are the limits of the customer's specifications.
Mechanical Properties
| Standard Equivalent | Erdemir Grade No | Re [N/mm2] | Rm [N/mm2] | Re/Rm | A(%) min. | n90 | r90 | |
|---|---|---|---|---|---|---|---|---|
| Standard | Quality | |||||||
| A80 | min. | |||||||
| 11-04-013 | XE | 312 | 180-230 | 300-370 | 0.74 max. | 34 | 0.17 | 1.3 min. |
- Tensile test values apply to "transverse" test pieces
- The mechanical properties are valid for a period of 6 months from the date on which the products are made available.
- Unless otherwise agreed, n value is taken between %10-20 elongation range.