6282 Quality Sheet Specification
Low and intermediate strength, atmospheric corrosion resistant structural steels
Reproducible Letter Symbols --> DS --> HRP --> HRPKK --> HRU --> HRUKK --> KRKK --> L --> LKK --> LP --> LPKK --> LR --> LRKK --> R --> RD --> RKK --> RP --> RPD --> RPKK --> THRU --> TR --> TRKK --> TRP
Flat / Hot Rolled
Flat steel products are obtained by heating semi-finished products with a rectangular cross-section (slab), which are produced by the continuous casting method, to a specific temperature and then rolling them, with thicknesses ranging from 1.40 to 25.40 mm and widths ranging from 700 to 2025 mm, produceed as coil or by cutting/slit-coiling flat steel products from coils.
Low and intermediate strength, atmospheric corrosion resistant structural steels
Chemical Composition (%)
| Standard Equivalent | Erdemir Grade No | Cmax. | Mnmax. | Pmax. | Smax. | Cumax. | Cumin. | |
|---|---|---|---|---|---|---|---|---|
| Standard | Quality | |||||||
| EN 10111:2008 | DD11 (Cu) | 6282 | 0.12 | 0.60 | 0.045 | 0.045 | 0.40 | 0.20 |
Mechanical Properties
| Standard Equivalent | Erdemir Grade No | Re [N/mm2] t(thickness, mm) | Rm [N/mm2] | A(%) min. t(thickness, mm) | ||||
|---|---|---|---|---|---|---|---|---|
| Standard | Quality | |||||||
| 1.5≤t≤1.99 | 2≤t≤11 | A801.5≤t≤1.99 | A802≤t≤2.99 | A53≤t≤11 | ||||
| EN 10111:2008 | DD11 (Cu) | 6282 | 170-360 | 170-340 | 440 max. | 23 | 24 | 28 |
- Tensile test values apply to "transverse" test pieces
- Recommended for use within 6 weeks from the date which products are made available.