6352 QualitySheet Specification

6352 Quality Sheet Specification

Hot rolled steels for pressure purposes (boilers, steam boiler plants, pressure vessels, etc.) at elevated temperatures

Reproducible Letter Symbols --> HRUKK --> KRKK --> L --> LKK --> LRKK --> RKK
Alternatives6335 6341 6347 6353

Flat / Hot Rolled

Flat steel products are obtained by heating semi-finished products with a rectangular cross-section (slab), which are produced by the continuous casting method, to a specific temperature and then rolling them, with thicknesses ranging from 1.40 to 25.40 mm and widths ranging from 700 to 2025 mm, produceed as coil or by cutting/slit-coiling flat steel products from coils.

Hot rolled steels for pressure purposes (boilers, steam boiler plants, pressure vessels, etc.) at elevated temperatures

Chemical Composition (%)

Standard EquivalentErdemir Grade NoThickness (mm)Cmin.Cmax.Mnmin.Mnmax.Pmax.Smax.Simax.Almin.Nmax.Crmax.Momax.Nimax.Vmax.Nbmax.Timax.Cumax.
StandardQuality
EN 10028-2:2017P355GH63521≤t≤60.100.220.901.700.0250.010.600.02120.000.300.080.300.020.040.030.30
EN 10028-2:2017P355GH63526.01≤t≤250.100.221.101.700.0250.010.600.02120.000.300.080.300.020.040.030.30
  1. Cu + Ni + Cr + Mo ≤ 0.70 %
  2. Al/N ≥ 2

Mechanical Properties

Standard EquivalentErdemir Grade NoRe [N/mm2] t(thickness, mm)Rm [N/mm2]A(%) min. t(thickness, mm)Impact
StandardQuality
1.8≤t≤1616.01≤t≤26A801.8≤t≤2.99A53≤t≤26Temperature ( ° C)6≤t≤7.49KVC J min.6≤t≤7.49Temperature ( ° C)7.5≤t≤9.99KVC J min.7.5≤t≤9.99Temperature ( ° C)10≤t≤26KVC J min.10≤t≤26
EN 10028-2:2017P355GH6352355 min.345 min.510-6502020-2014-2021-2027
  1. Tensile test values apply to "transverse" test pieces
  2. The tensile test for proof strength at elevated temperature is carried out on request.
  3. Impact test is not carried out for thickness thinner than 6 mm.
  4. Depending on agreement the impact energy can be specified as 40J in the purchase order.

Flat / Plate

Heavy plate products are obtained by rolling semi-finished products with a rectangular cross-section (slab) produced by the continuous casting method to a specific temperature, with thicknesses ranging from 6.00 to 200.00 mm and widths ranging from 1000 to 3600 mm.

Hot rolled steels for pressure purposes (boilers, steam boiler plants, pressure vessels, etc.) at elevated temperatures

Chemical Composition (%)

Standard EquivalentErdemir Grade NoCmin.Cmax.Mnmin.Mnmax.Pmax.Smax.Simax.Almin.Nmax.Crmax.Momax.Nimax.Vmax.Nbmax.Timax.Cumax.
StandardQuality
EN 10028-2:2017P355GH63520.100.221.101.700.0250.010.600.02120.000.300.080.300.020.040.030.30
  1. Cu + Ni + Cr + Mo ≤ 0.70 %
  2. Al/N ≥ 2

Mechanical Properties

Standard EquivalentErdemir Grade NoRe [N/mm2] t(thickness, mm)Rm [N/mm2]A(%) min.Impact
StandardQuality
6≤t≤1616.01≤t≤4040.01≤t≤50A5Temperature ( ° C)6≤t≤7.49KVC J min.6≤t≤7.49Temperature ( ° C)7.5≤t≤9.99KVC J min.7.5≤t≤9.99Temperature ( ° C)10≤t≤50KVC J min.10≤t≤50
EN 10028-2:2017P355GH6352355 min.345 min.335 min.510-65020-2014-2021-2027
  1. Tensile test values apply to "transverse" test pieces
  2. The tensile test for proof strength at elevated temperature is carried out on request.
  3. Impact test is not carried out for thickness thinner than 6 mm.
  4. Depending on agreement the impact energy can be specified as 40J in the purchase order.