6356 QualitySheet Specification

6356 Quality Sheet Specification

Dual certified hot rolled normalized fine grained steel suitable for pressure purposes

AlternativesThere is no alternative to this sheet.

Flat / Hot Rolled

Flat steel products are obtained by heating semi-finished products with a rectangular cross-section (slab), which are produced by the continuous casting method, to a specific temperature and then rolling them, with thicknesses ranging from 1.40 to 25.40 mm and widths ranging from 700 to 2025 mm, produceed as coil or by cutting/slit-coiling flat steel products from coils.

Dual certified hot rolled normalized fine grained steel suitable for pressure purposes

Chemical Composition (%)

Standard EquivalentErdemir Grade NoCmax.Mnmin.Mnmax.Pmax.Smax.Simax.Almin.Nmax.Crmax.Momax.Nimax.Vmax.Nbmax.Timax.Cumax.
StandardQuality
EN 10028-3:2017P355NH63560.181.101.700.0250.0080.500.02120.000.300.080.500.100.050.030.30
  1. Cu + Cr + Mo ≤ 0.45 %
  2. (Nb + V + Ti) ≤ 0.12%
  3. Al/N ≥ 2
  4. Minimum value for aluminium does not apply if the chemical composition includes additionally Nb, Ti or V.
  5. Suitable for dual certification.
  6. Depending on agreement, Cu + 6Sn ≤ 0,33 %

Mechanical Properties

Standard EquivalentErdemir Grade NoRe [N/mm2] t(thickness, mm)Rm [N/mm2]A(%) min. t(thickness, mm)Impact
StandardQuality
2.1≤t≤1616.01≤t≤26A802.1≤t≤2.99A53≤t≤26Temperature ( ° C)6≤t≤7.49KVC J min.6≤t≤7.49Temperature ( ° C)7.5≤t≤9.99KVC J min.7.5≤t≤9.99Temperature ( ° C)10≤t≤26KVC J min.10≤t≤26
EN 10028-3:2017P355NH6356355 min.345 min.490-6302222-4014-4021-4027
  1. Tensile test values apply to "transverse" test pieces
  2. The tensile test for proof strength at elevated temperature is carried out on request.
  3. Impact test is not carried out for thickness thinner than 6 mm.

Dual certified hot rolled normalized fine grained steel suitable for pressure purposes

Chemical Composition (%)

Standard EquivalentErdemir Grade NoCmax.Mnmin.Mnmax.Pmax.Smax.Simax.Almin.Nmax.Crmax.Momax.Nimax.Vmax.Nbmax.Timax.Cumax.
StandardQuality
EN 10028-3:2017P355NL163560.181.101.700.0250.0080.500.02120.000.300.080.500.100.050.030.30
  1. Cu + Cr + Mo ≤ 0.45 %
  2. (Nb + V + Ti) ≤ 0.12%
  3. Al/N ≥ 2
  4. Minimum value for aluminium does not apply if the chemical composition includes additionally Nb, Ti or V.
  5. Suitable for dual certification.
  6. Depending on agreement, Cu + 6Sn ≤ 0,33 %

Mechanical Properties

Standard EquivalentErdemir Grade NoRe [N/mm2] t(thickness, mm)Rm [N/mm2]A(%) min. t(thickness, mm)Impact
StandardQuality
2.1≤t≤1616.01≤t≤26A802.1≤t≤2.99A53≤t≤26Temperature ( ° C)6≤t≤7.49KVC J min.6≤t≤7.49Temperature ( ° C)7.5≤t≤9.99KVC J min.7.5≤t≤9.99Temperature ( ° C)10≤t≤26KVC J min.10≤t≤26
EN 10028-3:2017P355NL16356355 min.345 min.490-6302222-4014-4021-4027
  1. Tensile test values apply to "transverse" test pieces
  2. The tensile test for proof strength at elevated temperature is carried out on request.
  3. Impact test is not carried out for thickness thinner than 6 mm.

Flat / Plate

Heavy plate products are obtained by rolling semi-finished products with a rectangular cross-section (slab) produced by the continuous casting method to a specific temperature, with thicknesses ranging from 6.00 to 200.00 mm and widths ranging from 1000 to 3600 mm.

Dual certified hot rolled normalized fine grained steel suitable for pressure purposes

Chemical Composition (%)

Standard EquivalentErdemir Grade NoCmax.Mnmin.Mnmax.Pmax.Smax.Simax.Almin.Nmax.Crmax.Momax.Nimax.Vmax.Nbmax.Timax.Cumax.
StandardQuality
EN 10028-3:2017P355NH63560.181.101.700.0250.0080.500.02120.000.300.080.500.100.050.030.30
  1. Cu + Cr + Mo ≤ 0.45 %
  2. (Nb + V + Ti) ≤ 0.12%
  3. Al/N ≥ 2
  4. Minimum value for aluminium does not apply if the chemical composition includes additionally Nb, Ti or V.
  5. Suitable for dual certification.
  6. Depending on agreement, Cu + 6Sn ≤ 0,33 %

Mechanical Properties

Standard EquivalentErdemir Grade NoRe [N/mm2] t(thickness, mm)Rm [N/mm2]A(%) min.Impact
StandardQuality
6≤t≤1616.01≤t≤4040.01≤t≤50A5Temperature ( ° C)6≤t≤7.49KVC J min.6≤t≤7.49Temperature ( ° C)7.5≤t≤9.99KVC J min.7.5≤t≤9.99Temperature ( ° C)10≤t≤50KVC J min.10≤t≤50
EN 10028-3:2017P355NH6356355 min.345 min.335 min.490-63022-4014-4021-4027
  1. Tensile test values apply to "transverse" test pieces
  2. The tensile test for proof strength at elevated temperature is carried out on request.
  3. Impact test is not carried out for thickness thinner than 6 mm.

Dual certified hot rolled normalized fine grained steel suitable for pressure purposes

Chemical Composition (%)

Standard EquivalentErdemir Grade NoCmax.Mnmin.Mnmax.Pmax.Smax.Simax.Almin.Nmax.Crmax.Momax.Nimax.Vmax.Nbmax.Timax.Cumax.
StandardQuality
EN 10028-3:2017P355NL163560.181.101.700.0250.0080.500.02120.000.300.080.500.100.050.030.30
  1. Cu + Cr + Mo ≤ 0.45 %
  2. (Nb + V + Ti) ≤ 0.12%
  3. Al/N ≥ 2
  4. Minimum value for aluminium does not apply if the chemical composition includes additionally Nb, Ti or V.
  5. Suitable for dual certification.
  6. Depending on agreement, Cu + 6Sn ≤ 0,33 %

Mechanical Properties

Standard EquivalentErdemir Grade NoRe [N/mm2] t(thickness, mm)Rm [N/mm2]A(%) min.Impact
StandardQuality
6≤t≤1616.01≤t≤4040.01≤t≤50A5Temperature ( ° C)6≤t≤7.49KVC J min.6≤t≤7.49Temperature ( ° C)7.5≤t≤9.99KVC J min.7.5≤t≤9.99Temperature ( ° C)10≤t≤50KVC J min.10≤t≤50
EN 10028-3:2017P355NL16356355 min.345 min.335 min.490-63022-4014-4021-4027
  1. Tensile test values apply to "transverse" test pieces
  2. The tensile test for proof strength at elevated temperature is carried out on request.
  3. Impact test is not carried out for thickness thinner than 6 mm.